Blue coloration on stainless steel when subjected to heat

++++++

I wish to know what temperatures stainless steel pipe of grade AISI 316L has reached if blue spots are observed on pipe when it is subjected to heat in limited air atmosphere for a duration of 75 minutes.

ABHIJEET NANDEDKAR
MANUFACTURING - BHILAI, CHATTISGARH, INDIA


++++++

This is one of the weirdest thermometers I've ever heard of, Abhijeet :-)

Please provide the background and why you want to know. Thanks and good luck!

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


++++++

Hi Abhijeet,

I am sure you will find the answer at the Nickel Institute. Check out their web page www.nickelinstitute.org.

Have fun,

Tony Johnston
- Doncaster East, Melbourne, Australia


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search