Hi.
I'm looking for a simple process to polish tiny parts that cannot be polished mechanically.
The volume is low, there is no industrial scale production.
I know that a mix of acids and maybe other additives would do the job, but I don't know which and the proportions.
I would appreciate any help I can get.
Thanks,

Dan B.
Metal finishing - ON, Canada


++++++

You can use next solution:
10% phosphoric acid
10% hydrochloric acid
5% nitric acid
75% water
(80 C temp.,add 10 gm soot,5 minutes immersion)
Good luck!

Goran Budija
- Zagreb, Croatia


++++++

May I know that is it the above only suitable for 300series SS? How about 400series SS?

Leonard Yong
Precision (Hardware) - Singapore

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search