finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 39057

Electropolishing

++++++

Does Electropolish can enhance the surface finish of SS 316L ?

That is, is it decreasing the Ra value of the surface ?

Keshav Gokhale
Pharmalab - Ahmedabad, Gujarat, India


++++++

Yes, Keshav. But no more abstract questions, please. Instead, start by describing your situation. Thanks.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


++++++

WE ARE USING ELECTROPOLISHING FOR SS PART AS A CLEANING /SURFACE TREATENT & IT IS GIVING GOOD RESULT.

THOTE SHESHRAO
- AURANGABAD, INDIA


++++++

YES ELECTROPOLISHING IMPROVES ENHANCE FINISHING & RA VALUE IF PROPER CURRENT,TIME & CHEMICALS USED

SHESHRAO THOTE
- AURANGABAD, INDIA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search