I need to dull the burnished areas of an aluminum trailer

++++++

I cleaned graphics off of an aluminum tanker trailer. The spots where I scrubbed are now "polished". I do not want to buff out an entire trailer obviously. I just need to dull down the clean spots.

Kris Oliver
signs - Chillicothe, OH USA


++++++

You could always just use a little sandpaper, but that wouldn't ensure that the resulting finish would match the rest of the tanker, and it would probably remove any corrosion protection you have on the aluminum.

Have you tried using the search engine on this sight to search the archived letters? You may find that your situation has already been described and a solution given...

Good luck!

Jim Gorsich
Accurate Anodizing Inc.

Compton, California, USA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search