RoHS compliance plating

++++++

Hello,

Could someone tell me what RoHS compliance plating would be the best to replace Hard Anodize (Black color)?

John Ng
MFG. - Palo Alto, California


++++++

Umm, probably Hard Anodize. Who told you hard anodize wasn't RoHS compliant, and on what basis did they say it wasn't?

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


++++++

The only part of the anodizing process that MAY cause RoHS problems is the dye. If your dyeing, check with the dye manufacturer.

Justin Crisp
- Indianapolis, IN, USA


++++++

While I fully agree with both Ted and Justin, I remain puzzled about the source of the question. A very large computer manufacturer asked the same question having heard that black anodize is non-RoHS compliant! I'm assuming that this stems from the minor chromium content in SOME dyes, however, I'm not sure as to the valence state of the chromium in the dye, nor the level of chromium incorporated in the resultant coating. The fact that several people are confused on the subject might be cause for all users of black dye to go back to their manufacturers and get their dye manufacturer's "RoHS compliant declaration". The fact that there are so many black dyes to choose from might also complicate the issue if some are and some aren't.

Milt Stevenson, Jr.
Anoplate Corp

Syracuse, New York


++++++

The suppliers of our black dye and seal have certified them as RoHS complient.

Chris Jurey, President IHAA
Luke Engineering & Mfg. Co. Inc.

Wadsworth, Ohio


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search