Best material for pipeline to transport HF + HNO3

+++++

I want to construct a pipeline to transport HF & HNO3 for a pickling plant.
What material is best suitable to it.
also can you give me material for pipeline to transport KMNO4 , Lime, Phosphate & dilute HCL

Thank You

Abhishek Pande
Young Star Engineers - Nagpur, Maharashtra, India


+++++

Hi Abhishek,

Try PVC ... but you don't give any concentrations, nor pressure, nor temperature nor if the pipe is indoors, underground or exposed. Once those factors are known, one can make a more intelligent choice.

There are other plastics some violently expensive, however.

For the other line, presupposing abrasion from the lime, I'd opt for Polyethylene. This is available for low pressure applications and buried with 20' bell and spigot ends up to 10 feet or 12 feet diameter and even up to 5 feet diameter, heavy wall, for butt fusion ... I mean that's what's available over here ... and in Europe you can get 6 foot dia hdPe pressure pipe.

Freeman Newton - White Rock, British Columbia, Canada
Ed. note:
Please keep Freeman in your thoughts
& prayers.


Message from Freeman, Dec. 2010


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search