Need reliable plater for high-volume,
high-tech parts plating
+++++
I am consulting for a medium/high volume manufacturer of
electronics components. They have a series of components that are
suffering in quality due to poor plating. One part is tungsten and
one part is stainless. These need to be readily solderable.
Tungsten part currently has copper plate with tin on top for
antioxidant, and the SS part currently has nickel plate with tin on
top for antioxidant.
Current problem is that the tin surface is highly irregular (looks
like silver granola) and draws solder all over the place. We need a
nice finish to allow a better solder process to be implemented.
Michael S Forti
Electronics Mfg. - Virginia Beach, VA, USA
Dear Reader: Sorry, but there is no provision for public reply to
this particular letter because it appears to be a commercial inquiry
rather than a technical question. Our supporting advertisers should
reply privately.
- I want to see a list of current
letters where
public replies are welcomed.
-
- My company is a supporting advertiser at
finishing.com and we want the contact information to reach
the inquirer privately.
-
- Post a new
question on a different subject.
-
 |