What is the photoresist for the formula of etching Elgiloy?

+++++

We need a smooth through-etching of Elgiloy. The thickness is 0.15 to 0.25 mm. We find "How to etch Elgiloy (metal)?" in the following web:

http://www.finishing.com/119/36.shtml

15 mL HCl + 10 mL HNO3 + 10 mL acetic acid. Mix fresh. Swab onto the surface (Rather than immerse) for up to 4 minutes.

But it damages the photoresist. What type of photoresist that I should use?

Lu
- Minneapolis, USA


+++++

We have developed technology of etching Elgiloy without damaging photoresist. Contact us for samples treatment.


Anna Berkovich
Russamer Lab

Pittsburgh, Pennsylvania


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search