HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 38031
PLATING ISSUE
+++++
IF I SEND A SPEC. TO AN PLATER. IT SAYS ZINC DICHROMATE .00015-.0002 WHAT COLOR WILL THE PARTS COME BACK?
PAUL ADKINSELKINS MACHINE & TOOL - ROMULUS MICHIGAN
+++++
You have not specified, Paul, so they will come back whatever color the plater chooses based on convenience, economy, or his wish to give you additional corrosion protection. Maybe clear or blue, but just as likely yellow, less likely olive drab or black.
Some people think chromate means clear and dichromate means yellow, but I think that's an error with no support for it since chromate (CrO4) solutions are yellow and alkaline and dichromate (Cr2O7) solutions are orange and acidic. Please post your actual situation instead of a hypothetical and we can probably help more.
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |