Letter 37095
Basic course in electroplating
[India]
+++++
I'm a 3rd year student of BCS(computer science).
my uncle ownes a electroplating factory in nasik(maharashtra).
I'm interested in joining a short or a basic course that will help
join him at earliest.please help.
thank you.
Prathamesh Umesh Kulkarni
electroplating. - Nasik, Maharashtra
+++++
Mr. Kulkarni,
The Central Electrochemical Research Institute (CECRI) in Karaikudi,
Tamilnadu is organizing training courses on various topics including
electroplating and corrosion. See their website for more details.

T.S.N. Sankara Narayanan
- Chennai, Tamilnadu, India
+++++
Prathamesh,
Metal Finishing Association of India established in 1973 and a
premier organisation affiliated with IUSF(International Union for
Surface Finishing) coducts Certifiacte course in electroplating and
Metal Finishing every Year during April.This course has been
recognised by who is who in metal Finishing Industry in
India.Incidently I happened to be a member in the governing counsil
of this prestigiuos organsation for the last 6 years.Infact the
person who heads this certificate course Dr. Ashish Kulkarni lives in
Nasik,your native.
Prathamesh, Please try to be in Mumbai during 2-4 Feb 2006 for ISF
2006 where you can get plenty of knowledge in this promising
field
goodluck.
|
|
T.K. Mohan
plating process supplier
Mumbai, India
|
+++++
I'm not sure if the AESF is in India or not but I do know that
they offer a great beginners course for electroplateing. We use this
in our shop for all of our new platers I believe the cost is somthing
like $150.00(U.S.) you could check it out at www.aesf.com
Regards
Brian C. Gaylets
lock manufacturer - Scranton, Pennsylvania, U.S.A.
July 22, 2007
Pl give me the detais regarding to Diploma Courses for Plating.
Vivek Puranik
STI Sanoh India Ltd. - Dewas, M.P. , India
April 11, 2008
I'm interested in joining a short or a basic course that will help
join him at earliest.please help.
thank you,
SUNIL MADHAVRAO DENGLE
RAJ JEWELLERS - NASHIK, MAHARASTRA, INDIA
Dear Reader: please choose what you want to do--
- I want to answer or follow-up on this subject
publicly (in non-commercial
fashion).
-
- My company is a supporting advertiser at
finishing.com and we want the contact information to reach
the inquirer privately.
-
- I want to post a new
question or inquiry of my own on
a different subject.
-
 |