Protection against salt spray test on stainless steel

+++++

Hi, We are looking for any product or process (coating, plating or whatever) which can protect welded stainless steel parts (AISI630-X15TN) against 400H salt spray test. The parts need also to resist at 150° temperature.
Thank you for your earliest answers.

Simonetti Mivhele
automotive components producer - Pisa, Italy


+++++

High Phos electroless nickel gives 1000+ hours salt spray. Whether it is economical or feasible depends on your specific application.

Guillermo Marrufo
Monterrey, NL, Mexico
+++++

Hi Michele, electrophoretic coats have a high salt spray test resistance. Maybe try their resistance at high temp. if if fits your goal.

Dan L. Rujan
- Romania


+++++

Have you tried Autosol [linked by editor to product info at Amazon]? It is good for we tried the same for our aluminum and stainless steel salt spray test in enfield motor bikes.

M. Shanmugam
- Chennai, Tamil Nadu, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search