Letter 37075
Need to black oxide large hot rolled
steel [California]
+++++
I have ten large ornamental wall sculptures that range in
sizes:
approx. 3'5" x 4'5" and 4'5"x6'
made with 1/4"x1/2" flat bar
hot rolled steel
Six of the large ornamental wall sculptures can be viewed on the
internet at
www.goodhuevos.com/newsite
Click on Gallery, then Iron Doodles to see them.
I live in Northern California and have not been successful in finding
a shop who has big enough tanks to handle my pieces.
Isis Rodriguez
Professional Artist - San Francisco, CA, USA
Dear Reader: Sorry, but there is no provision for public reply to
this particular letter because it appears to be a commercial inquiry
rather than a technical question. Our supporting advertisers should
reply privately.
- I want to see a list of current
letters where
public replies are welcomed.
-
- My company is a supporting advertiser at
finishing.com and we want the contact information to reach
the inquirer privately.
-
- I want to post a new
question or inquiry of my
own.
-
 |
|