Letter 37063

ASTM Standards for NSS test on wheels [Turkey] 

+++++

Hi I'm Özge from Turkey. I've just graduated and newly started work. I'm a chemist. My company is producing wheels in Turkey. I want to make our Neutral Salt Spray corrosion test by myself. But I don't know what ASTM Standards apply for the wheels. What are the acceptable values for blisters and corrosion? Can I find original pictures about blister sizes? I found a copy but it's really hard to see. Sorry for my English. I'm waiting an answer to help me

Özge INÇUKUR
Chemist - Aydin, TURKEY


+++++

Hello Ozge.
You can purchase and download standards on-line at www.astm.org. Some general specifications are ASTM D610 [link is to spec at TechStreet] for degree of rusting and ASTM D714 [link is to spec at TechStreet] for evaluation of blister. These specifications typically do not specify pass/fail criteria, which is generally specified in engineering or material specifications.

Christa Lammers
National Exposure Testing

Sylvania, OH, USA


+++++

I would like to know the name of your wheel company and what you produce.

Roger Brodt
Long's Wheel & Rim - Jacksonville, Florida, USA


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com