Silkscreen on Anodize  

+++++

I would like to know what people think about silkscreening (for example a putting a part number) on an anodized surface. Is there a spec that would address this?

Sharise Phelps
manufacturer - Wichita, KS, USA


+++++

It will work fine if specified as part of the anodizing process. Silk screening that is integral to the anodizing won't come off even with sandpaper without a lot of effort. Silk screening on top of an anodized part probably won't be worth much.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    privacy policy    -    ©1995-2010 finishing.com