Brass gold plating  

+++++

Dear sir/madam :

we want to design a laser reflector . the substrate is brass and we want to plate gold on it . is there any underplate needed ( like nickel ) and how much the thickness should be .thanks for your assistance..

Iman.Vafaei
iman systems Co. - Tehran, IRAN


+++++

Yes, you need to do nickel plating on your brass prior to gold plating. Nickel works as an anti-diffusion layer between brass and gold. Copper and zinc will migrate to the top of the gold surface from bottom and get oxidized and black once they contact the air without having the brass nickel plated. 10-20 microns of nickel will be good enough.

Yunhan Kuo
- Thailand


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com