Which test for low performance plating on Steel parts?
+++++Hello,
I need to specify a test, that if passed would garantee that the parts will be able to remain White rust free after 2 years in an indoor environement (up to 95% humididty)
I tried some salt mist but 72 hours seems too severe.
Any recommendations ?