I have some 304 Stainless Sheet metal to be cleaned of some surface rust can I do this with Murodic Acid (Spelling ?)Sorry. can you make a recommendation the metal is installed, to cover insulation in a large Box approx. 6 mtr x 6 mtr.
Thanks for your help!

Marlyn Reed
- Preeyville, Arkansas


+++++

Don't even think about opening a bottle of Muriatic Acid [link is to product info at Amazon] upwind of this installation, Marlyn!

Buy a commercial stainless steel cleaner--which will most definitely not have any muriatic (hydrochloric) acid in it.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com