Gold plating pewter  

+++++

I have a pewter pendant that I would like to gold plate. Is that a special process such as nickel plating first? I was told by a relative that is fairly new to the industry that it could not be done. What are your thoughts, please.

Robert Bolles
Chassis R&D - Ormond Beach, FL USA


+++++

Yes, you could specify that the plating shop bright nickel plate and then gold plate the pendant if you wish. Without the nickel it would probably require an unaffordable amount of gold plating to get a bright finish. The pewter may need hydrofluoric acid activation, but that shouldn't be your problem either.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com