We are actually busy to design a meter in which there are steel terminals. At the moment, these terminals are plated with Zinc and Chromium. However, we have problems with this plating because chromium seems to be broken down by water and it reveals the Zinc plating which is able to be oxidated. That is why I would like to find other materials for this plating. Could you please give me information about other useable materials (cheaper than silver and gold, and having good electrical conductivity).

Samuel MERLET
Industrial Placement Trainee - Felixstowe, Suffolk, ENGLAND


+++++

0.0002" of bright nickel could be an alternative.

tom portrait
Tom Pullizzi
Falls Township, Pennsylvania


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search