44 hrs CASS CHROME

     

+++++

Hi,

I have a customer specified for 44hrs CASS Chrome finish with #400 grits. Can you let me where can I get the specs for 44 hrs CASS CHROME finish.

JACK LYNN
METCOR INDUSTRIES, INC. - WALNUT, California


August 11 +++++

CASS means copper-accelerated salt spray. So this is not a spec for the plating, but is a spec for the accelerated corrosion testing which the plating must survive. Look into spec ASTM B-368 [link is to spec at TechStreet].

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


+++++

If you are looking for a chrome plating spec that meets the 44 hours CASS test, try to get General Motors spec GM4374M. it is published with GM4372M and GM4373M. Also ASTM B456 [link is to spec at TechStreet] -03, SC 5.

Jim Vickers
- Concordville, Pennsyvania, USA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search