Chromium with Fluorine? and Chrome with 4% Silicone?

+++++

Gentlemen (or ladies),

I am a hard chrome plater and cater to the plastic injection mold industry. My customer has supplied me with an in-house specification for CRF. When I inquired as to what the specification was for, I was told it's chrome w/fluorine (Not Fluoride, but Fluorine). Could someone please give a general description of this coating? Could they be confusing this with a Fluoride catalyst hard chrome bath? Also, is chrome with 4% Silicone a wet chemistry or a PVD coating? Thank you for your assistance.

Love your site!

Jeff Hanaway
Injection Mold Plater - Meadville, Pennsylvania


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search