Need Plating on Plastic?
Try Here! -->
(Cycles thru suppliers)


Letter 36073

SEEKING CHROME PLATING OF MG37EP PLATABLE ABS PART  

+++++

Hello,

We are actively pursuing quotes for chrome plating of a platable ABS (GE Cycolac MG37EP) part. The part has a diamond buffed finish (mirror) on the cosmetic side. Size: 6.95" diameter, 1.45" high approximate surface area of cosmetic side 55 sq. in. A .stl file may be supplied upon request via email to purchasing. Initial order will be 250 parts and subsequent order (6 times yearly) will be 1000-2000 parts.

Joe Crawley
Manufacturing - Grand Rapids, Michigan


RFQ button

Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com