Dear Sir,

I am trying to find the method to make kinds of metal with red gold and white gole color from copper based. I want to make jewelry with lower prices than real gold or silver. After succeed in my experiences with your valuable advise, I will establish a company for my own, to make jewelry that is my hope for my family life.
I would like to present to you my problem as follow:
Can I mix copper with palladium to make white metal look like "with gold" for jewelry making ? Will it resitance with oxydice or corrosion ?
Please advise me the percentage of material(s).

With your valuable experiences, can you teach me the way to make "white gold" for jewelry ? Thank you in advance.

I am waiting to hear from you.

Sincerely yours,

Nguyen The Huy
HUNG NGUYEN CO, LTD. - HO CHI MINH, VIETNAM


October 3, 2008

I am trying to find the method to make kinds of metal with red gold and white gole color from copper based. I want to make jewelry with lower prices than real gold or silver. After succeed in my experiences with your valuable advise, I will establish a company for my own, to make jewelry that is my hope for my family life.

Look like "yellow gold" for jewelry making ? Will it resitance with oxydixe or corrosion ?

Please advise me the percentage of material(s).

Suresh Iyer
- India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search