HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 36000
Need Hard Ematal plating, preferably on 6061
+++++
I am familiar with Hard Ematal plating being applied to 5083 aluminum. I have a batch of 6061 aluminum plates I would like to have coated with Hard Ematal. Are there any compatability issues to be aware of using Hard Ematal on 6061? Also, are there any sources for Hard Ematal plating in the United States?
Thank you!
Gary WaltonLanco Assembly Systems, Inc. - Westbrook, Maine, USA
----
Readers: This site is made available for camaraderie & technical info exchange by our supporting advertisers, and they will contact the inquirer privately regarding their commercial needs. Please offer comments on any technical issues, but not sourcing suggestions or testimonials. Thanks!