Galvanising - Top Dross

        

+++++

What is Top Dross? How Top Dross is generated - How it differs from Bottom Dross ? Please mention the chemical composition.

S. R. Ameen
GALVANCO - Riyadh, Saudi Arabia


+++++

Assalamu Alikom,

You can have a quick look at the link below, you will find some answers to your questions through page 1 and 2 of the article, the rest is out of scope.

"http://products.teckcominco.com/Products/Technical_Documents/nachitechpaper.pdf"

Sameh Mohamed El Tahan
Kandil Industries - Cairo, Egypt


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search