Looking for a company that will chrome plastic parts

+++++

I have a few plastic parts on my car that I would like chromed. Is there a company that will do it in the U.S.?

Bernard Morrissey
Turner - Moorpark, California, USA

----
Ed. note: The following advertisers offer decorative chrome plating on plastic service:
 
 M&M Metalizing Sales [Westminster, CA] -- chrome-like vacuum metalizing
Miller Plating & Metal Finishing [Evansville, IN] -- industrial accounts only
Plating Technologies [Warren, MI]



----
Readers: This site is made available for camaraderie & technical info exchange by our supporting advertisers, and they will contact the inquirer privately regarding their commercial needs. Please offer comments on any technical issues, but not sourcing suggestions or testimonials. Thanks!


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search