Suitable sodium nitrite levels to inhibit corrosion

+++++

I work at an factory that sends aerosol cans through a water bath with sodium nitrite among other things to inhibit corrosion. Does anybody know what is the recommended concentration of sodium nitrite in ppm to use as a rust inhibitor. Couldn't find anything in print to include in my training manual.
Thank so much in advance.

Jim W [last name deleted for privacy by Editor]
quality assurance - Viburnum, Missouri


+++++

Dear Jim,

I am also interested in the responses you have received to your question.

Long ago, at a company I worked, we used to add sodium nitrite to prevent rust forming on pressure vessels put in water tank to perform pressure tests.

But I cannot remember the concentration. Now at another company I want to do same...

help / input would be appreciated.

Thanks

Stan p [last name deleted for privacy by Editor]
air conditioning - Staunton, Virginia


February 15, 2010

Nitrite level should be 1000-1500 ppm.

Thushara [last name deleted for privacy by Editor]
- Sri lanka

Corrosion and Corrosion Control


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search