Electrolytic stripping of electroless nickel-phosphorus coating

-

Does anyone have a formula for the electrolytic stripping of an electroless nickel-phosphorus coating?

warren silverman
- brooklyn ny


-

Please see our FAQs on Stripping of Electroless Nickel.

Regards,

 
Ted Mooney, P.E. - Finishing.com Inc. - Brick, NJ


.

My guess is that electrolytic stripping would needlessly etch the part that is probably being deposited with electroless nickel because there are precision tolerances which have been machined on it. I'd check out Metex non-cyanide processes or look into Meta-nitrobezoic acid (MNBA) I know that electrolytic stripping was accomplished using sulfuric acid, and in order to stop the etching the 'old tyme' platers put glycerine in it. But I'd still be wary of this.

Also from my experience with electroless nickel there is a black smut which develops on the part (as it strips) maybe an oxide of phosphorus?, put on rubber gloves and wipe or brush the part to accellerrate the stripping time. Sincerely Steve Wilcox

Steve Wilcox
- Tecumseh, Michigan


Dear Reader, please --

Answer or follow-up on this subject
 
Post a new question or inquiry on a different subject
 
This is a monitored forum. If you spot broken links or obsolete info, please advise!

 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com