Recycling N-propyl bromide

+++++

I have a customer who uses n-propyl bromide for part cleaning. Has anybody had any experience with recycling this material.

Thanks in advance.

Mark C. Reppa
- Plymouth, Michigan


++++++

Try WRR Environmental Services Eau Claire WI. A principal company which markets a n-propyl bromide product recommends this company for recycling/disposal.

Andy Fletcher
- San Francisco, California, USA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search