Descaling SS 310

+++++

I want to remove millscale (descale) SS 310 what should be the acids and proportions and how do I passivate and neutralise acid effect

Naresh Hinduja
Swan Enterprises Pvt. Ltd. - Chennai, Tamil nadu, India


+++++

Hello Naresh. Have you tried anything to date, and what were the results? Is a mechanical scale breaker part of the process, or no? Strong acid like nitric-hydrofluoric can be used, but the answer will be as vague as the question. Neutralization is usually just good rinsing followed by passivation, which can be with nitric acid or citric acid. Good luck.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search