Adhesion testing of printed characters on anodize  

++++

With regards to ASTM D 3363-00 Pencil Test. Is that test valid for testing adhesion of characters pad printed on an anodized metal surface? My impression is that the test is for a smooth painted surface only.

If there is a more preferred method for testing adhesion of characters printed on a surface, I'm all ears.

Thanks,

Bill Nibley
Manufacturing - Simi Valley, CA, USA


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com