Which kind of S.S. jacket for a pharma crystallizer

++++

Dear Sirs ,

We are a small company in Italy , producing stainless steel vessels only for pharma applications . Our range cover vessels with a "half pipe" jacket ,expecially used for medium / big size crystallizers needs to work both in pressure and vacuum .The question is : the client prod. needs to put inside the half pipe jacket steam at 3 or 4 bar ( 152°C ) and after couple of hours discharge the line and put inside the same jacket suddendly cold glicolate water ( 5°C ). They do two complete thermal cycle every day . What kind of S.S. do you suggest to use for jacket material , ( consider Aisi316L for the material in contact with the product ) in order to have as minimum elongation problems and cracs welds ?

Do you think Aisi304 can give any above mentionated problems and /or badly reactions .

We do MIG weld with a semi-autom . robot .

Tanks a lot in advance for your cooperation

Sincerely

Enrico Corradi
ILINOX S.R.L. - S.Polo, S.Polo - Parma, Italy


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search