I am a home owner and have inherited some silver candle sticks which have been converted into lamps. I am looking to find a way to somehow put a finish on the silver so that it doesn't tarnish. Is it possible to lacquer silver items which are decorative such as other metals like brass? (Using nail polish which was posted earlier seems impossible for larger items).Thank you for any help or resources.

Irene Vale
Homeowner - Auburn, WA, USA


++++

Yes, you can lacquer your silver. You can use 75 gm Paraloid B 72 resin(or 44 or 67)/1 lit toluene solution. Or try to find Frigilene lacquer.

Good luck!

Goran Budija
- Zagreb , Croatia


++++

Agateen lacquer is also very good (USA product)!

Good luck!

Goran Budija
- Zagreb , Croatia


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search