Creating thin film of MgB2 by sol-gel method

++++

I am interested in synthesis of MgB2 thin films by sol-gel process starting prefeably from Mg- acetate and Boric acid. Please suggest me the route.

Dr. Sujit Kumar Bandyopadhyay
Variable Energy Cyclotron Centre - Kolkata, West Bengal, India


September 15, 2008

I am interested too in synthesis of MgB2 thin films by sol-gel process, but I donot find any paper in this subject. if you find paper about it please send me too.I am starting reaserch on fabrication of MgB2 thin films by spray method. If I succsess inform you

Fahimeh Abrinaey
IAU university - Tehran, Iran


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
Post a new question or inquiry on a different subject.
 

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search