NIKASIL

-

PLEASE SEND TO ME FOR WORK IN MAY SCHOOL ABOUT COMPOSITION COVER BATH NIKASIL....I AM STUDENT QUIMICA ...

HELOISA TURCI
STUDENT - ARARAQUARA BRAZIL


-

I believe that you are referring to a proprietary, composite, nickel/silicon carbide deposit.

This is a coating formed by nickel electroplating where silicon carbide particles are present in the bath, and codeposit in the coating as the nickel is being electrochemically reduced at the surface of the part. You may want to start your research under the non-proprietary topic of composite plating.

Regards,

Tom Pullizzi
platronica.com
Falls Township, PA 

 


+

Please I am needing information for application of Nikasil (Silicon-Carbide) Patent, formulates etc.

Luiz Paulo Agostini
- Bento GonÁalves, RS, Brazil


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com