We are trying to do passivation of 15-5 PH steel & 17-4 PH steel with HNO3 + HF [3:1]solutions. The results are not so encouraging since overetching of surface is taking place.

Request to suggest most suitable process for passivation of these steels. Can Phosphoric acid + Chromic acid or Nitric acid + Sodium Dichromate process be used for these steel? Which is most suitable?

Biren Desai
Godrej & Boyce Mfg. Co. Ltd. - Mumbai, Maharashtra, India


++++

Biren,

Take a look at QQ-P-35 [link is to info about spec at TechStreet] for the proper method to passivate 17-4PH and 15-5PH Stainless Steel.

Tim Hamlett
Techno Coatings, Inc. - Miami, Florida


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com