Letter 32088
Process on powdercoating alumium products
++++
Dear Sir:
I have a question about powdercoat on Alumium. We have 1,000 pcs
of alumium products ,for which we are going to powdercoat them matt
black. However they were undertaking chemical reaction when
phosphating. As major in steel and stainless steel,we are
inexperienced in this field. Could you please give us a few
suggestions?
Best Regards,
David Wei
metal fabrication - Xiamen, Fujian, China
++++
Although it is possible to put zinc phosphate on aluminum, it is
not possible to iron phosphate aluminum. You have not given us any
details, so we have no idea whether there is a minor flaw in your
sequence or you are attempting something that is hopeless from the
start. It is probably better to chromate the aluminum than to
phosphate it.
You need to either retain a consultant or to align yourself with a
powder coating supplier and a pretreatment supplier who know what
they are doing. Good luck.
|
|

Ted Mooney, P.E.
finishing.com
Brick, New Jersey
|
Dear Reader, please --
- Answer or follow-up on this subject (in non-commercial
fashion).
-
- My company is a supporting advertiser at
finishing.com and we want the contact information to reach
the inquirer privately.
-
- Post a new
question or inquiry on a different subject.
-
 |