Letter 32067 ++++ Hello, My husband and I have been selling fabulous and unique 1950's era
chrome dinette sets for many years now. We restore tables and chairs
as needed and have always had exceptional results using the process
of applying chrome polish to buff out areas after removing any rust
or corrosion, albeit we tend to avoid any chrome in this condition.
However, where needed we find that it just takes a lot of elbow
grease to obtain optimal results restoring these wonderful tables,
chairs and dinette sets to their original state. Roxanne C
I would love to know where we can buy replacement feet for our
1950's chrome dinette set, especially the table legs. They are the
double legs that are curved at the top and joined at the bottom, so
we need something similar to a figure 8 to place at the bottom of the
chrome to protect the floor. Any help will be appreciated. Thanks Kimee L
Where do I find a place to do replating? I live in the Bay
Area. Ben H Ed. note: There are some plating shops in the Bay area listed
in our Directory of Jobshops, Ben.
Good luck.
I have a 1950's Retro Chrome red metalic dinette set(I think a
Douglass) with curved legs and I am missing one of the 8 legs. Where
can I get replacement legs? Janice M

![]()
- San Jose, CA, USA
Roxanne: chrome polish and elbow grease is an affordable and
practical approach in many cases. But once there has been rust, it
means the chrome is perforated--and polishing it doesn't repair it,
it remains a high maintenance issue with only regular polishing and
rewaxing limiting the rusting. Although replating is rather expensive
expensive, that's the way to truly restore the set to original
condition. You might want to align yourself with a local plating shop
so you have this option.
Ted Mooney, P.E.
finishing.com
Brick, New Jersey
+++++
![]()
- Orangevale, CA
+++++
Thanks,![]()
- Albany, CA, USA
+++++++
Thanks,![]()
- Bellerose, N.Y., USA
Dear Reader, please --

Save
This Page (why?) - Home - ©1995-2009 finishing.com