Looking for a way to discolor nickel [Pennsylvania] 

++++

Hello.

I have an older (1970's vintage) electric guitar. I am updating the hardware, but I would like the hardware to retain a "vintage" appearance. The older guitras all had nickel-plated steel hardware (most newer guitars have chrome-plated hardware). I am looking for a way to prematurely age the new nickel-plated hardware I have purchased for this guitar. I have seen vintage instruments with original discolored nickel hardware, and it really adds to the appearance. I know that letting sterling silver contact cooked egg yolks will hasten the tarnishing process (by adding a disproportionate amount of sulphur to its environment); does the same hold true for nickel?

Many thanks in advance for a reply.

Daniel Klasnick
musician hobbyist - Pittsburgh, PA, U.S.A.


++++

The chrome plating on top of the nickel, if present, must be stripped first. Then the nickel will tarnish and yellow by itself. I don't think eggs will speed it up, but no harm trying.

 
Ted Mooney, P.E.
finishing.com Inc. - Brick, NJ


++++

If the nickel is allowed to be exposed tothe atmosphere, it will naturally tarnish. This can be enhanced by exposing it it an atmosphere rich in either hydrogen sulphide or sulphur dioxide. Both gases will produce a dark grey/black thin coating of nickel sulphide. Eggs may well do the trick, but could take some time.

Trevor Crichton
R&D practical scientist - UK


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com