Where to get Copper Nitrate  

++++

Where can I find copper nitrate? Can anyone recommend something else to rust or patine mild steel... Thanks in advance...

Corby Allbright
- Naples, Fl, Usa


++++

Copper nitrate is available from chemical supply houses, but they may not wish to sell to artists, or have appropriate size containers for that purpose, since they probably usually ship palettes of four 55-gal drums.

For smaller quantities you might want to try Bryant Laboratory [Berkeley, CA]..


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


++++

Any chemist can make you copper nitrate by dissolving copper wire in nitric acid.


Cair Shishani

aircraft maintenance - Abu Dhabi, UAE


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com