What is QQ-N-290 Grade G
++++
Can anyone tell me what
QQ-N-290 [link is to spec at TechStreet], Class 1, Grade
G represents. I cannot get through on the astimage web site. Need
immediately. Many thanks!
Todd West
Importer - Sebastian, FL, USA
++++
QQ-N-290, Class 1, Grade G represents a 0.0002 inch (5 micron)
nickel plating. It can be used for copper and copper-rich alloys
(< 40% zinc).
QQ-N-290 is in fact still available from the ASSIST site, as are
many other canceled specifications [just click on the document icon].
Download any of foreseeable use, since future availability is
uncertain.
|
Ken Vlach
- Goleta, California
|
|