I'm trying to compare the mechanical properties of three different materials, one of the test I conducted was a tensile test. My problem is that the three materials are of different thicknesses, is there any way of still relating the results I obtain from the tests?

Gboyex Ake
plating - London, England


++++

Tensile strength is expressed per unit of cross-sectional area, so the thickness of the material is already taken into account in rating the tenisle strength. But other than noting that, your question is to vague for me to understand.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


++++

Tensile testing can be carried out on an Instron instrument and there are set procedures for its operation. These should be followed and you will have directly comparible results. As Ted says, the tensile strength is related to cross sectional area, so, if you do not use standard test specimens, you can take this into account when doing the calculations. I think you need to give more detail of exactly what you are doing before you will get any definitive replies.

Trevor Crichton
R&D practical scientist - UK


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com