Cycles thru suppliers.


Letter 31071

Best metal mix for our continuous galvanizing line process  

++++

AS A GI MAKER I HAVE FOUND YOUR WEGSITE EXTREMELY INTERESTING. MY QUESTION IS:

1./REFERRING TO THE ZN POT IN CONTINOUS GALVANIZING LINE WHAT ROLE CAN PLAY THE FOLLOWING CHEMICAL ELEMENT AND WHAT IS BEST PERCENTAGE OF THEM : Pb, Sb, Al

2./WHAT IS THE BEST AND THE MOST EFFECTIVE WAY TO CHECK-MEASURE AND CONTROL THE TEMPERATURE OF STEEL STRIP INSIDE THE NOF FURNACE.

THANKS FOR YOUR ANSWER.

TRAN THE AI
GI MAKER - THUAN AN, BINH DUONG, VIETNAM


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com