Letter 31024
Looking for a blackening compound
equivalent to BLACKER-4929
++++
We are making socket set screws.We use High Alloy Steels for
making these products.All these products are heat treated to achieve
the desired mechanical properties.After heat treatment, the
blackening compound is used for rust preventive coating as a mixture
of water and compound and after the tempering operation the fasteners
are dropped into the blackening compound through a conveyor. The
ratio of the compound is maintained by measuring the PH level.
We understand that some of our Indian manufacturers of these items
are using BLACKER-4929 OF NIPPON GREASE CO. LTD.,JAPAN. We infact are
looking for a blackening compound equivalent to BLACKER-4929 OF
NIPPON GREASE.
Presently we are not using any blackening compound instead,
achieve BLACK COLOUR by lowering the temperature in the tempering
furnace to 160 degree centigrade to 170 degree centigrade but we are
not able to get the optimum colour and surface coating is also not as
good as in Taiwanese products.
Hence in order to achieve surface finish and rust preventive
coating same as of Taiwanese products.We are looking for a blackening
compound equivalent to BLACKER-4929 or superior then it if possible
as to what blackening compound they are using . Please help us in
this matter and arrange to sent Technical Literature.
Looking forward for your early reply.
With best regards,
Naveen
- India
Dear Reader: Sorry, but there is no provision for public reply to
this particular letter because it appears to be a commercial inquiry
rather than a technical question. Our supporting advertisers should
reply privately.
- I want to see a list of current
letters where
public replies are welcomed.
-
- My company is a supporting advertiser at
finishing.com and we want the contact information to reach
the inquirer privately.
-
- Post a new
question on a different subject.
-
 |