Letter 3065

Low Chrome Seal For Anodized Aluminum 

-

I am interested in a "low chrome" 125 ppm dichromate seal for anodized aluminum. Where might I find technical information on this process? Is such a seal formulation proprietary or patented?

Steven Hendricks
- Fort Worth, Texas


-

The aerospace industry uses such a seal and it is not proprietary. The seal composition is contained in Boeing and Mac specs., BAC5019 Chromic Acid Anodize, but the solution is made up and maintained to the following limits: Hex chrome 45-100ppm as Cr+6, pH 3.2-3.8, Silicates 10ppm max., TDS max., 250ppm. The temp used for processing depends upon if the low voltage(22v) or high(40v) voltage process is used.The makeup is 26g/100gal chromic acid with 18g/100gal sodium chromate using DI water.

Ward Barcafer, CEF
aerospace - Wichita, Kansas


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com