Letter 3036 Palladium chloride as a pre-cursor for silver deposition- Could anybody assist me with information regarding successive process steps of stannous chloride then palladium chloride as a pre-cursor to silver deposition on non-conductive substrates? David Bamber
- This can probably be done, but it is an unusual mixing of technologies. There are three different wet processing technologies that are commonly used to metallize non-conductors. 1). Applying a two-part silver reduction system. In this approach, a soluble silver salt and a reducing agent are simultaneously sprayed onto the substrate to deposit metallic silver. This is done as the first step in making stampers for vinyl records. 2). Applying a colloidal suspension of conductive granules, which can be graphite, copper, or silver. This is more or less painting the part with a conductive silver paint, and is often used to metallize flowers, leaves, and things like that. 3). The palladium chloride / stannous chloride system which is used to precede electroless copper or electroless nickel deposition on plastics, for use on such things as automotive brightwork. I suppose it is possible to follow routine #3 with electroless copper, followed by electrolytic copper, and then electrolytic silver. However, this is done (to my knowledge) exclusively with proprietary sequences. You might want to talk to Enthone/OMI, Atotech, Shipley, or MacDermid. I think you would also find the book "Standards and Guidelines for Electroplated Plastics" to be a big help.
Dear Reader: please choose what you want to do.
![]() |
|
Save
This Page (why?) - Home - ©1995-2008 finishing.com