Quantum Magnetics needs a small quantity (less than 10 meters) of Permalloy-plated Cu-Be wire of diameter .005" -.015". This wire will be used in support of magnetic sensing experiments. It would be great if a plating company in southern California (or anywhere in USA) could help us. Regards, Charlie