HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 30060
What is annual usage of zinc, nickel, and copper for plating?
++++I am a student trying to find out how many metric tons of zinc, nickel and copper are used each year in the U.S.A for electroplates?
Leslie Tstudent - San Diego, California, USA
I think you have the order right, so that's a good start. I would be inclined to believe that zinc, nickel, and copper are respectively #1, #2, and #3 in usage. You might call around to plating shops and see if any have the Surface Finishing Market Research Board reports that cover this. Good luck.
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |