finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 30037

Ready-made test kit for checking SS316?

++++

We have a few SS316 materials fabricated and machined. There is no scope for cutting a sample to check the chemical composition. Also we are not in a position to go for handheld tester to test these materials as they are simply not available at the place of material. Is there any other method by which I can check the material.

Thanks,

G Y SRINIVAS
Engineering - DELHI, INDIA


Having now seen handheld X-ray fluorescence "scrap sorters", G.Y., I'm sure it's the best way to go, although very expensive -- in excess of $20,000 U.S.

For other less expensive methods such as you seek, please patiently apply the search engine and you will find that the question has already been asked and answered repeatedly. For example, letters 5505, 6060, 16172, 18574, 23766, and 40586 are a good start. Good luck!

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search