HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => letter 30032
EN plating shop needs info on the Armalloy [Armoloy®] TDC process
++++
I need to know something about "armalloy tdc" process.
PIERO D [last name deleted for privacy by Editor]plating enp shop - MILAO, ITALY
May , 2010
Hi, Piero. I can tell you that "TDC" is an acronym for "Thin Dense Chrome", Piero, and that the correct spelling of the brand is Armoloy®. Hopefully this is enough that you'll be able to durther research it. Good luck.
Regards,
|